DIN EN ISO 7539-6
Corrosion of metals and alloys - Stress corrosion testing - Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement (ISO 7539-6:2018, Corrected version 2018-11 + Amd 1:2024); German version EN ISO 7539-6:2018 + A1:2024
Korrosion der Metalle und Legierungen - Prüfung der Spannungsrisskorrosion - Teil 6: Vorbereitung und Anwendung von angerissenen Proben für die Prüfung unter konstanter Last oder konstanter Auslegung (ISO 7539-6:2018, korrigierte Fassung 2018-11 + Amd 1:2024); Deutsche Fassung EN ISO 7539-6:2018 + A1:2024
Overview
This document specifies procedures for designing, preparing and using precracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of precracked specimens for investigating susceptibility to stress corrosion. Recommendations concerning notched specimens are given in Annex A. The term "metal" as used in this document includes alloys. Because of the need to confine plasticity at the crack tip, precracked specimens are not suitable for the evaluation of thin products, such as sheet or wire, and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding. The responsible national standardization committee is Working Committee NA 062-01-77 AA "Korrosionsprüfverfahren" ("Corrosion testing") at DIN Standards Committee Materials Testing (NMP).
Responsible national committee
NA 062-01-77 AA - Corrosion testing